Customization: | Available |
---|---|
Usage: | Concrete, Filling Material, Spinning, Non-Woven Fabric, Fabric |
Material: | 100% Polyester |
Still deciding? Get samples of US$ 1.2/kg
Request Sample
|
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
Tested Item | Unit | Standard | |
Value | Tolerance | ||
Size,Denier, Linear Density | dtex | M | ±3% |
Tensile Strength, Tenacity | Cn/dtex | 3,5< | |
Tenacity CV | max:6% | ||
Extension Percentage, Elongation | % | 22 | ±3 |
Elongation CV | max: 8% | ||
Crimp Shrinkage, Crimp Contraction Shirinkage at elasticity |
% | 16 | ±3 |
Crimp Modul (CM) | % | 12 | ±3 |
Cripmp Stability, Stability of elasticity (CS) | % | 85 | ±3 |
Shrinkage at Boiling Water | % | 2 | ±1 |
Shrinkage at hot air | % | 5 | ±2 |
Interlace | p.p.m. | HIM 90-120, SIM:75-110 | ±10 |
Stability at %3 elengation | % | ||
Stability at %5 elengation | % | HIM min 95%, SIM max:50 | |
Oil-bearing Ratio | % | 2.0 | ±0,5 |
Dyeing Evenness, Dying affinity testing apparatus(gray card) garding |
Grade | 4.5 |